Trumpet-Wood vs Balsa

Cecropia peltata against Ochroma pyramidale. Every number below names the publication it came from.

PropertyTrumpet-WoodBalsa
Janka hardness320 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)88 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC23.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)11.5 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture6,490 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)3,140 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity1.09 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)0.49 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength3,490 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)2,160 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)8.3%Chudnoff 1984, Tropical Timbers of the World (AH-607)10.8%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)3.10Chudnoff 1984, Tropical Timbers of the World (AH-607)2.53USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.