Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Tuturubá vs Abiurana

Pouteria gongrijpii = Franchetella gongrijpii against Pouteria sp. Every number below names the publication it came from.

PropertyTuturubáAbiurana
Janka hardness2,396 lbfLPF/SFB Madeiras Brasileiras2,418 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC56.9 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-957.4 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture20,951 lb/in²LPF/SFB Madeiras Brasileiras22,516 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.22 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.45 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras
Crushing strength10,952 lb/in²LPF/SFB Madeiras Brasileiras11,436 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)15.0%LPF/SFB Madeiras Brasileiras15.2%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)2.24LPF/SFB Madeiras Brasileiras1.64LPF/SFB Madeiras Brasileiras

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.