Tuturubá vs Abiurana

Pouteria oblanceolata against Pouteria guianensis. Every number below names the publication it came from.

PropertyTuturubáAbiurana
Janka hardness2,923 lbfLPF/SFB Madeiras Brasileiras2,921 lbfLPF/SFB Madeiras Brasileiras
Density at 12% MC59.9 lb/ft³LPF/SFB Madeiras Brasileiras58.7 lb/ft³LPF/SFB Madeiras Brasileiras
Modulus of rupture22,217 lb/in²LPF/SFB Madeiras Brasileiras20,382 lb/in²LPF/SFB Madeiras Brasileiras
Modulus of elasticity2.23 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras—
Crushing strength11,293 lb/in²LPF/SFB Madeiras Brasileiras9,871 lb/in²LPF/SFB Madeiras Brasileiras
Volumetric shrinkage(lower is better)13.8%LPF/SFB Madeiras Brasileiras13.3%LPF/SFB Madeiras Brasileiras
Tangential / radial ratio(lower is better)1.71LPF/SFB Madeiras Brasileiras1.76LPF/SFB Madeiras Brasileiras

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.