Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Ucuúba / virola vs Banak

Virola multicostata against Virola spp.. Every number below names the publication it came from.

PropertyUcuúba / virolaBanak
Janka hardness496 lbfLPF/SFB Madeiras Brasileiras510 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Density at 12% MC35.5 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-936.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture8,250 lb/in²LPF/SFB Madeiras Brasileiras10,900 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Modulus of elasticity1.45 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.04 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Crushing strength5,504 lb/in²LPF/SFB Madeiras Brasileiras5,140 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b
Volumetric shrinkage(lower is better)—13.7%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4
Tangential / radial ratio(lower is better)3.25LPF/SFB Madeiras Brasileiras1.91USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • GWDD v2.2 (Fischer et al. 2026)CC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.