Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Ucuubarana vs Kirikawa

Iryanthera grandis against Iryanthera spp.. Every number below names the publication it came from.

PropertyUcuubaranaKirikawa
Janka hardness1,195 lbfLPF/SFB Madeiras Brasileiras930 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC48.9 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-935.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture15,432 lb/in²LPF/SFB Madeiras Brasileiras12,650 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity1.81 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras2.18 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength8,662 lb/in²LPF/SFB Madeiras Brasileiras6,970 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)13.5%LPF/SFB Madeiras Brasileiras15.6%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)1.61LPF/SFB Madeiras Brasileiras1.77Chudnoff 1984, Tropical Timbers of the World (AH-607)

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.