White Cypress-Pine vs Longleaf pine

Callitris glauca against Pinus palustris. Every number below names the publication it came from.

PropertyWhite Cypress-PineLongleaf pine
Janka hardness1,375 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)870 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Density at 12% MC42.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)41.3 lb/ft³USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Modulus of rupture11,400 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)14,500 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Modulus of elasticity1.30 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)1.98 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Crushing strength7,610 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)8,470 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Volumetric shrinkage(lower is better)—12.2%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3
Tangential / radial ratio(lower is better)—1.47USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3

Sources

  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3public domain
  • USDA FIA REF_SPECIESpublic domain
  • GWDD v2.2 (Fischer et al. 2026)CC BY 4.0

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.