Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Xixá vs Sterculia

Sterculia excelsa = Sterculia speciosa against Sterculia pruriens. Every number below names the publication it came from.

PropertyXixáSterculia
Janka hardness1,071 lbfLPF/SFB Madeiras Brasileiras798 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC39.4 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-937.0 lb/ft³Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of rupture13,764 lb/in²LPF/SFB Madeiras Brasileiras9,700 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Modulus of elasticity1.80 ×10⁶ lb/in²LPF/SFB Madeiras Brasileiras1.93 ×10⁶ lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Crushing strength7,159 lb/in²LPF/SFB Madeiras Brasileiras8,230 lb/in²Chudnoff 1984, Tropical Timbers of the World (AH-607)
Volumetric shrinkage(lower is better)16.2%LPF/SFB Madeiras Brasileiras15.4%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)2.04LPF/SFB Madeiras Brasileiras2.11Chudnoff 1984, Tropical Timbers of the World (AH-607)

Sources

  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.