Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Young-growth redwood vs White oak

Sequoia sempervirens against Quercus alba. Every number below names the publication it came from.

PropertyYoung-growth redwoodWhite oak
Janka hardness420 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b1,360 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Density at 12% MC24.5 lb/ft³USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b47.6 lb/ft³USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Modulus of rupture7,900 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b15,200 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Modulus of elasticity1.10 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b1.78 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Crushing strength5,220 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b7,440 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Volumetric shrinkage(lower is better)7.0%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-316.3%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3
Tangential / radial ratio(lower is better)2.23USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-31.88USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3public domain
  • manual map (regional variant)public domain
  • GWDD v2.2 (Fischer et al. 2026)CC BY 4.0
  • USDA FIA REF_SPECIESpublic domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.