Black maple vs Red maple

Acer nigrum against Acer rubrum. Every number below names the publication it came from.

PropertyBlack mapleRed maple
Janka hardness1,180 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b950 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Density at 12% MC39.8 lb/ft³USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b37.8 lb/ft³USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Modulus of rupture13,300 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b13,400 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Modulus of elasticity1.62 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b1.64 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Crushing strength6,680 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b6,540 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3b
Volumetric shrinkage(lower is better)14.0%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-312.6%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3
Tangential / radial ratio(lower is better)1.94USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-32.05USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-3bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-3public domain
  • USDA FIA REF_SPECIESpublic domain
  • GWDD v2.2 (Fischer et al. 2026)CC BY 4.0