Wood Record

Compare two woods

Choose any two species to compare their published properties. Search by common or scientific name. Your selections stay in the URL, ready to share.

Sucupira vs Canalete

Diplotropis purpurea against Cordia spp. (hard-wooded, dark-colored Gerascanthus group). Every number below names the publication it came from.

PropertySucupiraCanalete
Janka hardness2,140 lbfUSDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b2,200 lbfChudnoff 1984, Tropical Timbers of the World (AH-607)
Density at 12% MC56.2 lb/ft³LPF/SFB Madeiras Brasileiras58.2 lb/ft³EstimateUSDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9
Modulus of rupture20,600 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b—
Modulus of elasticity2.87 ×10⁶ lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b—
Crushing strength12,140 lb/in²USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5b—
Volumetric shrinkage(lower is better)11.8%USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-411.6%Chudnoff 1984, Tropical Timbers of the World (AH-607)
Tangential / radial ratio(lower is better)1.52USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-41.85Chudnoff 1984, Tropical Timbers of the World (AH-607)

Sources

  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 5-5bpublic domain
  • USDA Wood Handbook 2021 (FPL-GTR-282) Table 4-4public domain
  • LPF/SFB Madeiras BrasileirasCC BY 4.0
  • USDA Wood Handbook 2021 (FPL-GTR-282) eq. 4-9public domain
  • Chudnoff 1984, Tropical Timbers of the World (AH-607)public domain

Estimates are labeled beside their values. A dash means no published value is available. Properties describe the source material; individual boards vary.

All comparisons

Published comparisons

400 selected pairs, each with a published Janka test for both woods.