Wood Record

All wood species

1,785 species. 571 carry a published Janka test. A species with no test says so.

1,785 matching species · Estimates are marked with an asterisk. Images may show a related species; see credits.

Wood species and selected properties
WoodRegionWood typeJanka hardnessDensity
‘a‘mati‘e

Elaeocarpus floridanus

Genus image · Cirad · Public domain
Range not recordedhardwood915 lbf*37.1 lb/ft³*
Abacatirana

Ocotea aciphylla = Ocotea costulata

Genus image · Cirad · Public domain
Tropical Americahardwood1,025 lbf38.7 lb/ft³
Abata cola

Cola acuminata

Genus image · Cirad · Public domain
Range not recordedhardwood1,419 lbf*45.5 lb/ft³*
Abiu-branco

Pouteria oppositifolia

Genus image · Cirad · Public domain
Tropical Americahardwood1,788 lbf*50.7 lb/ft³*
Abiurana

Pouteria anomala

Genus image · Cirad · Public domain
Tropical Americahardwood2,472 lbf56.2 lb/ft³
Abiurana

Pouteria sp

Genus image · Cirad · Public domain
Tropical Americahardwood2,418 lbf57.4 lb/ft³
Abiurana

Pouteria egregia

Genus image · Cirad · Public domain
Tropical Americahardwood2,950 lbf67.7 lb/ft³*
Abiurana

Pouteria guianensis

Cirad · Public domain
Tropical Americahardwood2,921 lbf58.7 lb/ft³
Abiurana-branca

Pouteria caimito

Genus image · Cirad · Public domain
Tropical Americahardwood2,608 lbf56.8 lb/ft³
Abiurana-branca

Micropholis mensalis

Genus image · Cirad · Public domain
Tropical Americahardwood1,605 lbf46.2 lb/ft³
Abiurana-mangabarana

Micropholis guyanensis

Genus image · Cirad · Public domain
Tropical Americahardwood1,781 lbf48.7 lb/ft³
Abiurana-seca

Diploon cuspidatum = Diploon venezuelana

Tropical Americahardwood2,945 lbf68.7 lb/ft³*
Abura

Mitragyna ciliata

Africahardwood780 lbf34.0 lb/ft³
Aceitillo

Pilocarpus racemosus

Range not recordedhardwood3,647 lbf*70.6 lb/ft³*
Aceitillo falso

Simarouba tulae

Genus image · Cirad · Public domain
Range not recordedhardwood1,309 lbf*43.8 lb/ft³*
Achiotillo

Alchornea latifolia

Genus image · Cirad · Public domain
Range not recordedhardwood753 lbf*33.9 lb/ft³*
Açoita-cavalo

Lueheopsis duckeana

Genus image · Cirad · Public domain
Tropical Americahardwood1,767 lbf48.9 lb/ft³*
Adoung

Monopetalanthus heitzii

Cirad · Public domain
Africahardwood542 lbf*33.0 lb/ft³
Afa

Neonauclea forsteri

Cirad · Public domain
Range not recordedhardwood1,419 lbf*45.5 lb/ft³*
Afina

Strombosia glaucescens

Genus image · Cirad · Public domain
Africahardwood2,963 lbf*61.0 lb/ft³
African Blackwood

Dalbergia melanoxylon

Cirad · Public domain
Africahardwood—83.0 lb/ft³
African Canaríum

Canarium schweinfurthii

Cirad · Public domain
Africahardwood670 lbf30.0 lb/ft³
African Celtis

Celtis spp.

Genus image · Cirad · Public domain
Africahardwood1,670 lbf45.0 lb/ft³
African Corkwood

Musanga cecropioides

Cirad · Public domain
Africahardwood165 lbf*18.0 lb/ft³
African ebony

Diospyros spp.

Genus image · Cirad · Public domain
Africahardwood3,220 lbf63.0 lb/ft³
African Homalium

Homalium spp.

Genus image · Cirad · Public domain
Africahardwood2,050 lbf54.0 lb/ft³
African mahogany

Khaya spp.

Genus image · Cirad · Public domain
Africahardwood830 lbf32.0 lb/ft³
African Padauk

Pterocarpus soyauxii

Cirad · Public domain
Africahardwood1,538 lbf*46.0 lb/ft³
African Pencil Cedar

Juniperus procera

Cirad · Public domain
Africasoftwood717 lbf*36.0 lb/ft³
African sumac

Rhus lancea

Genus image · Cirad · Public domain
Range not recordedhardwood818 lbf*35.2 lb/ft³*
African tuliptree

Spathodea campanulata

Cirad · Public domain
Range not recordedhardwood395 lbf*25.1 lb/ft³*
African-Walnut

Lovoa trichilioides syn. L klaineana

Cirad · Public domain
Africahardwood940 lbf34.0 lb/ft³
Afrormosia

Pericopsis elata

Cirad · Public domain
Africahardwood1,560 lbf43.0 lb/ft³
Afzelia

Afzelia spp.

Genus image · Cirad · Public domain
Africahardwood1,810 lbf51.0 lb/ft³
Agba

Gossweilerodendron balsamiferum

Cirad · Public domain
Africahardwood740 lbf30.0 lb/ft³
Aguacatillo

Meliosma herbertii

Cirad · Public domain
Range not recordedhardwood915 lbf*37.1 lb/ft³*
Aidia racemosa

Aidia racemosa

Genus image · Cirad · Public domain
Range not recordedhardwood2,367 lbf*57.7 lb/ft³*
Ailanthus

Ailanthus altissima

Cirad · Public domain
Range not recordedhardwood791 lbf*34.7 lb/ft³*
Akee

Blighia sapida

Cirad · Public domain
Range not recordedhardwood2,139 lbf*55.1 lb/ft³*
Alahee

Psydrax odorata

Cirad · Public domain
Range not recordedhardwood2,448 lbf*58.7 lb/ft³*
North Americahardwood——
Albarco

Cariniana spp.

Genus image · Cirad · Public domain
Tropical Americahardwood1,020 lbf35.0 lb/ft³
Albizzia

Albizia spp.

Genus image · Cirad · Public domain
Africahardwood955 lbf40.0 lb/ft³
Aleppo pine

Pinus halepensis

Genus image · Cirad · Public domain
Range not recordedsoftwood599 lbf*32.3 lb/ft³*
Alerce

Fitzroya cupressoides

Mark Wagner · CC BY 4.0
Tropical Americasoftwood560 lbf30.0 lb/ft³
Alexandra palm

Archontophoenix alexandrae

Forest & Kim Starr · CC BY-SA 3.0
Range not recordedhardwood2,779 lbf*62.2 lb/ft³*
Alexandrian laurel

Calophyllum inophyllum

Cirad · Public domain
Range not recordedhardwood1,255 lbf*43.0 lb/ft³*
Allegheny chinkapin

Castanea pumila

Genus image · Cirad · Public domain
Range not recordedhardwood573 lbf*29.8 lb/ft³*
Allegheny plum

Prunus alleghaniensis

Genus image · Cirad · Public domain
Range not recordedhardwood832 lbf*35.5 lb/ft³*
Allegheny serviceberry

Amelanchier laevis

Robert H. Mohlenbrock · Public domain
Range not recordedhardwood1,852 lbf*51.5 lb/ft³*
Alligator juniper

Juniperus deppeana

Genus image · Cirad · Public domain
Range not recordedsoftwood717 lbf*36.3 lb/ft³*
Alligatorwood

Guarea glabra

Genus image · Cirad · Public domain
Range not recordedhardwood1,309 lbf*43.8 lb/ft³*
Allspice

Pimenta dioica

Genus image · Cirad · Public domain
Range not recordedhardwood3,441 lbf*68.7 lb/ft³*
Aloalo

Premna serratifolia

Cirad · Public domain
Range not recordedhardwood1,007 lbf*38.8 lb/ft³*
Alom

Melanolepis multiglandulosa

Range not recordedhardwood479 lbf*27.5 lb/ft³*
Alstonia

Alstonia congensis

Cirad · Public domain
Africahardwood410 lbf25.0 lb/ft³
Amapa amargoso

Parahancornia fasciculata = Parahancornia amapa

Cirad · Public domain
Tropical Americahardwood789 lbf35.0 lb/ft³
Amapá-doce

Brosimum parinarioides

Genus image · Cirad · Public domain
Tropical Americahardwood1,250 lbf43.8 lb/ft³*
Amapá-doce

Brosimum potabile

Cirad · Public domain
Tropical Americahardwood1,184 lbf40.5 lb/ft³*
Amate

Ficus obtusifolia

Genus image · Cirad · Public domain
Range not recordedhardwood608 lbf*30.7 lb/ft³*
Amburana

Amburana cearensis

Cirad · Public domain
Tropical Americahardwood790 lbf42.1 lb/ft³*
Amendoim

Pterogyne nitens

Jorge Vallmitjana · Public domain
Tropical Americahardwood1,852 lbf*50.0 lb/ft³
American basswood

Tilia americana

Genus image · Roger Culos · CC BY-SA 4.0
North Americahardwood410 lbf25.8 lb/ft³
North Americahardwood1,300 lbf44.8 lb/ft³
American chestnut

Castanea dentata

Genus image · Cirad · Public domain
North Americahardwood540 lbf30.1 lb/ft³
American elm

Ulmus americana

Genus image · Cirad · Public domain
North Americahardwood830 lbf35.0 lb/ft³
American holly

Ilex opaca

Genus image · Cirad · Public domain
North Americahardwood960 lbf*38.0 lb/ft³*
American hornbeam

Carpinus caroliniana

Genus image · Cirad · Public domain
Range not recordedhardwood1,363 lbf*44.7 lb/ft³*
American mountain-ash

Sorbus americana

Genus image · Cirad · Public domain
Range not recordedhardwood1,103 lbf*40.5 lb/ft³*
American muskwood

Guarea guidonia

Cirad · Public domain
Range not recordedhardwood1,363 lbf*44.7 lb/ft³*
American plum

Prunus americana

Genus image · Cirad · Public domain
Range not recordedhardwood832 lbf*35.5 lb/ft³*
American sycamore

Platanus occidentalis

Famartin · CC BY-SA 4.0
North Americahardwood770 lbf34.3 lb/ft³
Range not recordedhardwood1,363 lbf*44.7 lb/ft³*
Amescla

Trattinnickia burserifolia

Cirad · Public domain
Tropical Americahardwood697 lbf35.5 lb/ft³*
Amoora

Amoora spp.

Genus image · Cirad · Public domain
Asiahardwood895 lbf46.0 lb/ft³
Amora / amoreira

Maclura tinctoria

Cirad · Public domain
Tropical Americahardwood2,385 lbf56.8 lb/ft³
Amur corktree

Phellodendron amurense

Bruce Marlin · CC BY 3.0
Range not recordedhardwood679 lbf*32.3 lb/ft³*
Range not recordedhardwood1,363 lbf*44.7 lb/ft³*
Range not recordedhardwood1,475 lbf*46.4 lb/ft³*
Amur maple

Acer ginnala

Genus image · Cirad · Public domain
Range not recordedhardwood832 lbf*35.5 lb/ft³*
Anacahuita Texas Olive

Cordia boissieri

Genus image · Cirad · Public domain
Range not recordedhardwood1,203 lbf*42.1 lb/ft³*
Anacua knockaway

Ehretia anacua

Genus image · Cirad · Public domain
Range not recordedhardwood1,419 lbf*45.5 lb/ft³*
Anadenanthera peregrina

Anadenanthera peregrina

Cirad · Public domain
Range not recordedhardwood2,064 lbf*54.2 lb/ft³*
Andaman Padauk

Pterocarpus dalbergioides

Cirad · Public domain
Asiahardwood1,630 lbf48.9 lb/ft³*
Andira-uxi

Andira surinamensis = Andira retusa

Genus image · Cirad · Public domain
Tropical Americahardwood1,788 lbf43.7 lb/ft³
Andiroba

Carapa guianensis

Cirad · Public domain
Tropical Americahardwood1,130 lbf41.0 lb/ft³
Angélica

Dicorynia paraensis

Cirad · Public domain
Tropical Americahardwood946 lbf36.2 lb/ft³
Tropical Americahardwood725 lbf31.0 lb/ft³
Angelim

Hymenolobium sp

Genus image · Cirad · Public domain
Tropical Americahardwood1,422 lbf44.9 lb/ft³
Angelim / angelim-rajado

Zygia racemosa = Marmaroxylon racemosum

Cirad · Public domain
Tropical Americahardwood3,177 lbf61.8 lb/ft³
Angelim-amargoso

Vatairea sericea

Genus image · Cirad · Public domain
Tropical Americahardwood2,167 lbf56.2 lb/ft³
Angelim-pedra

Hymenolobium modestum

Genus image · Cirad · Public domain
Tropical Americahardwood1,647 lbf50.7 lb/ft³*
Angelim-pedra

Hymenolobium petraeum

Cirad · Public domain
Tropical Americahardwood1,301 lbf44.3 lb/ft³
Angelim-pedra

Hymenolobium pulcherrimum

Genus image · Cirad · Public domain
Tropical Americahardwood1,206 lbf44.3 lb/ft³
Angelim-pedra

Hymenolobium nitidum

Genus image · Cirad · Public domain
Tropical Americahardwood1,257 lbf43.1 lb/ft³
Angelim-tinto

Andira sp

Genus image · Cirad · Public domain
Tropical Americahardwood1,989 lbf56.2 lb/ft³
Angelim-vermelho

Dinizia excelsa

Cirad · Public domain
Tropical Americahardwood3,045 lbf66.9 lb/ft³*
Angelin

Andira inermis

Cirad · Public domain
Africahardwood1,750 lbf52.0 lb/ft³
Angelique

Dicorynia guianensis

Cirad · Public domain
Tropical Americahardwood1,290 lbf50.0 lb/ft³
Angico

Peltogyne cf subsessilis

Genus image · Cirad · Public domain
Tropical Americahardwood2,941 lbf60.6 lb/ft³

Browse by botanical classification

Genera (286)
Families (105)